Please use this identifier to cite or link to this item: http://repositorio.ufla.br/jspui/handle/1/48070
Title: Effect of elevated temperature on sisal fibers degradation and its interface to cement based systems
Keywords: Torrefaction
Natural fibers - High temperatures
Natural fibers - Decomposition
Natural fibers - Adhesion
Natural fibers - Bonding
Natural fibers - Spalling
Torrefação
Fibras naturais - Altas temperaturas
Fibras naturais - Decomposição
Fibras naturais - Adesão
Fibras naturais - Fragmentação
Issue Date: 22-Feb-2021
Publisher: Elsevier
Citation: FERREIRA, S. R. et al. Effect of elevated temperature on sisal fibers degradation and its interface to cement based systems. Construction and Building Materials, Guildford, v. 272, 121613, 22 Feb. 2021. DOI: 10.1016/j.conbuildmat.2020.121613.
Abstract: This experimental investigation aims to study the influence of temperature on natural fibers mechanical performance and on its interface to cement based systems. Natural sisal fiber was used on this study. Temperatures of 20, 100, 150, 200, 250 and 300 °C were used as conditions for this research. The influence of temperature on this fiber was evaluated by scanning electron microscopy (SEM), x-ray diffraction patterns (XRD), thermogravimetric analysis (TGA). The mechanical properties were evaluated by tensile test. Pullout test were performed in order to evaluate bonding on cement-based matrix after exposition to higher temperatures. The results indicate a minor modification on sisal morphology after temperature exposition until 200 °C. At 250 °C a few microcracks were observed on fiber surface, indicating a debonding of sisal fibercells and microfibrils. Sisal mechanical behavior was improved until 150 °C. This may happen due the water evaporation and shrinkage, promoting a closed and densified fiber structure. Cement main component degradation was observed before degradation of the natural fiber (around 250 °C). Bonding to cement matrix decreased after 100 °C and was maintained stable until 150 °C, and resulted in pullout forces reduction of 75% in comparison to fiber tested at 20 °C.
URI: https://doi.org/10.1016/j.conbuildmat.2020.121613
http://repositorio.ufla.br/jspui/handle/1/48070
Appears in Collections:DEG - Artigos publicados em periódicos

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.