Please use this identifier to cite or link to this item: http://repositorio.ufla.br/jspui/handle/1/49270
Title: Produção e caracterização de compósitos à base de gesso reforçado com partículas de resíduo da agroindústria do cacau
Other Titles: Production and characterization of gypsum-based composites reinforced with cocoa agroindustry waste particles
Keywords: Resíduo lignocelulósico
Absorção de água
Resistência térmica
Materiais compósitos
Lignocellulosic waste
Water absorption
Thermal resistance
Composite materials
Issue Date: 12-Mar-2021
Publisher: Universidade Federal do Rio de Janeiro (UFRJ)
Citation: VELOSO, M. C. R. de A. et al. Produção e caracterização de compósitos à base de gesso reforçado com partículas de resíduo da agroindústria do cacau. Matéria, [S.l.], v. 26, n. 1, p. 1-16, 2021. DOI: 10.1590/S1517-707620210001.1245.
Abstract: This work aimed to produce and characterize gypsum-based composites reinforced with cocoa waste particles as a way to add value to this agricultural by-product and create an innovative material. For the production of composites, thin plaster for casting and particles of cocoa waste were used. The reinforcement proportions inserted were 0.0%; 2.5%; 5.0%; 7.5% and 10.0% replacing plaster mass. For the production of composites, wooden molds with dimensions of 40 x 40 x 160 mm were used. Analysis of the chemical composition of the cocoa waste was performed to determine the levels of total extracts, ash, lignin and holocellulose. The composites were evaluated in physical, mechanical, thermal and acoustic tests. It was found that there were improvements in physical properties with the addition of reinforcement making the material lighter, given the reduction in density (1190.69 to 1138.92 kg/m³), ??and providing a decrease in hygroscopicity, with moisture levels decreasing from 7.74 to 4.01% and water absorption decreasing from 18.37 to 5.28%. Likewise, the thermal resistance gradually increased over the treatments with values ??from 1.90 to 2.41 K.m/W and the acoustic insulation was higher in composites compared to pure plaster, although there was no linearity between treatments. As for the mechanical properties, there was a decrease in resistance both to flexion (3.60 to 0.84 MPa) and to compression (4.43 to 1.73 MPa). It was concluded that the cocoa waste has the potential to be used in the composite considering that the inclusion of up to 8.15% of the same met the standard in all tests performed. This promotes the idea that lignocellulosic waste is a promising alternative for creating materials with high added value.
URI: http://repositorio.ufla.br/jspui/handle/1/49270
Appears in Collections:DEG - Artigos publicados em periódicos



This item is licensed under a Creative Commons License Creative Commons