Use este identificador para citar ou linkar para este item: http://repositorio.ufla.br/jspui/handle/1/31841
Registro completo de metadados
Campo DCValorIdioma
dc.creatorSantos, Amélia S. F.-
dc.creatorPereira-da-Silva, Marcelo A.-
dc.creatorOliveira, Juliano E.-
dc.creatorMattoso, Luiz H. C.-
dc.creatorMedeiros, Eliton S.-
dc.date.accessioned2018-11-20T10:30:21Z-
dc.date.available2018-11-20T10:30:21Z-
dc.date.issued2016-06-
dc.identifier.citationSANTOS, A. S. F. et al. Accelerated sonochemical extraction of cellulose nanowhiskers. Journal of Nanoscience and Nanotechnology, [S.l.], v. 16, n. 6, p. 6535-6539, June 2016.pt_BR
dc.identifier.urihttps://www.ingentaconnect.com/content/asp/jnn/2016/00000016/00000006/art00168%3bjsessionid=dqadgl4vqpsa.x-ic-live-02pt_BR
dc.identifier.urihttp://repositorio.ufla.br/jspui/handle/1/31841-
dc.description.abstractStudies on sonochemical hydrolysis of cellulose have been suggested as an alternative route to obtaining cellulose nanoparticles. In this work, the potential use of acid hydrolysis assisted by sonication to obtain cellulose whiskers was studied. Parameters such as acid concentration, hydrolysis time and temperature were investigated to evaluate their effect on the morphological properties of the nanowhiskers, as compared to the conventional extraction process by acid hydrolysis with mechanical stirring. Morphology and degree of crystallinity of the nanowhiskers were studied by atomic force microscopy (AFM) and X-ray diffraction (XRD). Results indicated that the extraction time was reduced from about 45 min to less than 3 min using the same acid concentration and temperature used in conventional acid hydrolysis treatment. Likewise, it was possible, within the range of 30 min, to extract whiskers at room temperature or using half the concentration of acid by raising the temperature to about 80 °C. These are promising results towards a more economically viable and ecologically friendly extraction procedure used to obtain cellulose nanowhiskers, since both extraction time and acid concentration, used in nanowhisker extraction, were significantly reduced by replacing mechanical with sonochemical stirring.pt_BR
dc.languageen_USpt_BR
dc.publisherAmerican Scientific Publisherspt_BR
dc.rightsrestrictAccesspt_BR
dc.sourceJournal of Nanoscience and Nanotechnologypt_BR
dc.subjectCellulosept_BR
dc.subjectHydrolysispt_BR
dc.subjectNanowhiskerspt_BR
dc.subjectSonicationpt_BR
dc.titleAccelerated sonochemical extraction of cellulose nanowhiskerspt_BR
dc.typeArtigopt_BR
Aparece nas coleções:DEG - Artigos publicados em periódicos