Please use this identifier to cite or link to this item: http://repositorio.ufla.br/jspui/handle/1/33924
Full metadata record
DC FieldValueLanguage
dc.creatorLopes, Thamirys Andrade-
dc.creatorBufalino, Lina-
dc.creatorClaro, Pedro Ivo Cunha-
dc.creatorMartins, Maria Alice-
dc.creatorTonoli, Gustavo Henrique Denzin-
dc.creatorMendes, Lourival Marin-
dc.date.accessioned2019-04-27T10:47:34Z-
dc.date.available2019-04-27T10:47:34Z-
dc.date.issued2018-09-
dc.identifier.citationLOPES, T. A. et al. The effect of surface modifications with corona discharge in pinus and eucalyptus nanofibril films. Cellulose, [S.l.], v. 25, n. 9, p. 5017–5033, Sept. 2018.pt_BR
dc.identifier.urihttps://link.springer.com/article/10.1007/s10570-018-1948-3pt_BR
dc.identifier.urihttp://repositorio.ufla.br/jspui/handle/1/33924-
dc.description.abstractThe corona treatment is promising for the improvement of the quality of fabrics and composites, but there are only a few studies on its effectiveness for surface modification of nanofibril films for printing and packaging purposes. This investigation aimed to evaluate the effect of the evolution of corona discharge exposition on the superficial, physical and mechanical properties of eucalyptus and pinus nanofibril films. Cellulose nanofibrils were produced from commercial bleached cellulose pulps after 30 passages in a SuperMasscolloider Grinder. Films were formed by a casting method. The corona discharge treatment was applied for 10, 30, 60, and 300 s at a distance of 3 cm. Furthermore, the duration of the surface modification was evaluated after 6, 24, 48, 72, and 96 h. The corona discharge promoted the formation of hydroxyl, carbonyl, and other functional groups by breaking C–C bonds and their subsequent reaction with oxygen. The best corona treatment time was 30 s, for which maximum water vapor permeability of 13.1 and 14.2 g mm/KPa day m2 was found for the eucalyptus and pinus films, respectively. In addition, maximum water absorption (of around 35%) was observed for films of both genera treated for 30 s. The tensile strength increased in response to increasing corona treatment exposition. Pinus nanofibril films showed better performance than eucalyptus nanofibril films due to their higher crystalline index and nanofibril dimensions. Through the analysis of contact angle and surface energy, it was verified that printing of corona treated nanofibril films should be carried out for up to 24 h when the films still exhibit the treatment effect.pt_BR
dc.languageen_USpt_BR
dc.publisherSpringerpt_BR
dc.rightsrestrictAccesspt_BR
dc.sourceCellulosept_BR
dc.subjectBleached cellulose pulpspt_BR
dc.subjectWater vapor permeabilitypt_BR
dc.subjectSurface energypt_BR
dc.subjectDurabilitypt_BR
dc.titleThe effect of surface modifications with corona discharge in pinus and eucalyptus nanofibril filmspt_BR
dc.typeArtigopt_BR
Appears in Collections:DCF - Artigos publicados em periódicos

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.